Pack-Off Failure Investigation

During drilling, a section of drill pipe unexpectedly failed. This pipe was a rental, and we were asked to determine what had happened.

It was immediately clear to us that the failed end had been highly heated. It had deformed before it failed and separated. This indicated to us that this was a pack-off failure.

A pack-off is a condition where the formation being drilled has a series of hard material layers with soft layers above them. The bore in the hard material is on gauge, and the bore in the soft material opens up larger. The harder cuttings escape into the larger soft bore and pack around the pipe, gripping the pipe and causing a friction stop. In this instance, the friction was enough that a weak section of piping fractured, causing the failure.

In this photograph, the twisting of the hot pipe before fracture is visible.

Pack off Failure

Leave a Reply

Fill in your details below or click an icon to log in:

WordPress.com Logo

You are commenting using your WordPress.com account. Log Out / Change )

Twitter picture

You are commenting using your Twitter account. Log Out / Change )

Facebook photo

You are commenting using your Facebook account. Log Out / Change )

Google+ photo

You are commenting using your Google+ account. Log Out / Change )

Connecting to %s